ʻO ka hoʻonā ʻana i nā hemahema maʻamau o ka hoʻoheheʻe ʻia ʻana

He mea maʻamau nā hemahema i ka wā e hoʻohana ai i nā mold e hoʻoponopono i nā ʻāpana hoʻoheheʻe plastic injection, a pili kēia i ka hana pono. ʻO nā hemahema maʻamau a me nā hoʻonā no nā ʻāpana mold injection plastic.
Nā pana pōkole
ʻO nā kiʻi pōkole e pili ana i nā huahana i hana ʻia ʻaʻole i hoʻopiha ʻia ma muli o ka piha ʻole ʻana o nā mold.
ʻIke pinepine ʻia kēia hemahema ma kahi mamao loa mai ka ʻīpuka a i ʻole nā ʻāpana hiki ke loaʻa wale ma nā wahi haiki o ka ʻōpala no ka mea e pili ana nā wahi haiki i ke kahe o ka hehee.
Hiki i ka pana pōkole ke kumu i nā hōʻailona micro flow a i ʻole ka hopena i kahi hapa nui o ka huahana i nalowale maopopo.
Ke kumu:
ʻO nā kumu no nā kiʻi pōkole:
ʻAʻole lawa ka mea maka i hoʻokomo ʻia i loko o ka mol.
ʻO ke kū'ēʻana o nā melts he nui, no lailaʻaʻole hiki ke hoʻopiha pihaʻia ka'ōmole.
ʻAʻole maikaʻi ka hoʻoheheʻe ʻana o ka ʻeleʻele a ke kumu i ka hoʻokumu ʻana o ka cavitation e ālai i ka heheʻe, ʻaʻole hiki ke kahe ka hehee i kekahi mau wahi o ka pala.
Nahenahe
Hoʻokumu ʻia nā burrs mai ka hoʻopili ʻana o nā mea maka i hoʻokuʻu ʻia mai ka lua mold a i ka huahana.
Aia kēia hemahema ma nā ʻaoʻao o ka huahana a i ʻole kēlā me kēia ʻāpana i haku ʻia. Hiki ke hoʻopiha ʻia ka mea maka mai ka poʻi, a i ʻole nā wahi hoʻopaʻa o ka neʻe a me ka hoʻoponopono ʻana.
Hiki ke ʻike ʻia nā burrs ma ke kumu mold, ma muli o ke kaomi hydraulic a i ʻole ka pine angular.
ʻOkoʻa ka paʻakikī o nā burr, i kekahi manawa lahilahi, i kekahi manawa ʻoi aku ka mānoanoa.
Ke kumu:
ʻO nā kumu o ka burrs penei:
Ua pōʻino a ʻeha nui paha ka ʻili o ka pipili.
Hoʻokaʻawale ʻia ka ʻōpala neʻe a me ka hoʻoponopono ʻana i ka wā i laka ʻia.
ʻOi aku ka kiʻekiʻe o ke kaomi o ka mea maka i loko o ka mold ma mua o ka ikaika clamping mold.
ʻO ke kolu o ke ʻano i ʻōlelo ʻia ma luna nei ma muli o nā kumu like ʻole. I kēia mau kūlana, ʻoi aku ka kiʻekiʻe o ke kaomi o ka mea maka ma mua o ka ikaika clamping mold.
I ka pae mua o ka injection mold (mold filling stage), nui loa ka mea maka i hoʻopiha ʻia, e hoʻonui ai i ke kaomi i loko o ka mold.
I ka wā o ka hoʻopiha piha ʻana, ʻo ke kūʻē nui o ka kahe hehee e hoʻokiʻekiʻe i ke kaomi i loko o ka mold.
Kiʻekiʻe loa ke kaomi ʻana o ka lua i ka wā o ka paʻa ʻana o ke kaomi.
ʻAʻole lawa ka ikaika o ka hoʻopili ʻana.
Pauki
Hiki i ka decomposition ke alakaʻi i nā hopena he nui. ʻOkoʻa ka nui a me ka paʻakikī o ka pilikia. I ka hihia koʻikoʻi loa, hiki ke hoʻopau i ka ʻeleʻele piha o ka huahana a me nā waiwai mechanical maikaʻi ʻole. ʻO ka hoʻohaʻahaʻa kūloko e hoʻoulu wale i nā kaha ʻeleʻele a i ʻole nā kiko.
Ke kumu:
ʻO ka hoʻohaʻahaʻa ke kumu i ka pōʻino o ka mea maka. ʻO nā molekole kaulahao lōʻihi e hana i nā plastics e pohō ma lalo o ka hana o ka wela nui a i ʻole ke koʻikoʻi ʻoki nui. I ka wā o ka hoʻoheheʻe ʻana o nā molekala, e wikiwiki ke kinoea volatile i ke kaʻina hana hoʻohaʻahaʻa, kahi e hoʻoheheʻe ʻia ai ka mea maka. ʻO ka decomposition o ka nui o nā molekala e wāwahi hope i ka ʻike o ka mea maka a hoʻoulu i ka hopena maikaʻi ʻole i nā waiwai mechanical.
Hiki ke ho'oha'aha'a ka'āina ma muli o ka wela like 'ole o ka pahu mea.
Hiki ke hoʻohaʻahaʻa i nā kūlana ma lalo nei:
Hoʻomaʻamaʻa ʻia ka mea maka i loko o ka pahu waiwai a i ʻole ka ʻōnaehana holo wela.
Noho ka mea maka i loko o ka barela no ka lōʻihi loa.
I ka wā o ke kaʻina hana hoʻoheheʻe ʻia, ʻoi aku ka nui o ke koʻikoʻi o ka shear ma luna o ka mea maka. Inā paʻa nā nozzles, a haiki paha nā ʻīpuka a me ke kukini, e hoʻonui ia i ke koʻikoʻi ʻā.
Hoʻolaha
I nā kūlana maʻamau, pono ke ʻano o nā huahana e like me ke ʻano o nā mold. ʻO ka deformation e pili ana i ka deformity o nā huahana.
Ke piʻi aʻe ka maʻi, e hoʻopau loa ʻia nā huahana i ka wā e hoʻokuʻu ʻia ai mai ka ʻōpala. Inā ʻaʻole koʻikoʻi ke kūlana, e ʻike ʻia ke ʻano o ka huahana i nā hewa liʻiliʻi.
ʻO ka lōʻihi akā ʻaʻohe ʻaoʻao kākoʻo a i ʻole nā mokulele nui nā wahi i maʻalahi loa i ka deformation.
Ke kumu:
Nā kumu o ka deformation:
He kiʻekiʻe loa ka mahana i ka wā e hoʻokuʻu ʻia ai ka poʻo.
ʻOiai ʻokoʻa ka manawa hoʻoluʻu ma nā wahi mānoanoa a lahilahi, a i ʻole ka ʻokoʻa o ka mahana o ka mold i ka neʻe ʻana a me ka hoʻoponopono ʻana i ka pala, ʻokoʻa ka emi ʻana o nā huahana.
ʻAʻole maʻalahi ke kahe ʻana o ka mold i ka hoʻopiha ʻana (ʻo ia ka mea i kapa ʻia ʻo "Freezing orientation") a i ʻole ke kiʻekiʻe o ke kaomi ʻana i loko o ka lua polū ma ke kahua paʻa paʻa.
Nā Pāʻai
Hōʻike pinepine ʻia nā mea haumia ma ke ʻano o nā kiko i nā kala like ʻole, nā ʻāpana a i ʻole nā kaha. ʻO ka mea maʻamau ka wahi ʻeleʻele.
He mau kiko liʻiliʻi wale nō paha nā mea haumia, akā hiki ke ʻike ʻia nā ʻōpala a i ʻole ka hapa nui o ka kala ʻana ke koʻikoʻi.
Ke kumu:
Hoʻokumu ʻia nā mea haumia e nā mea i hui pū ʻia me nā mea maka, e like me:
ʻO ka mea maka i hui pū ʻia me nā mea like ʻole ke lawe ʻia i loko o nā barela.
Hiki ke hāʻule ka decomposition o ka mea maka mai nā mīkini ʻoki a hui ʻia i loko o nā mea maka, e like me nā bolts mīkini, ka paia o loko o ka pahu maloʻo, nā hono / nozzles.
Lami
ʻO ka lamination e hoʻoulu i ka "hopena ʻili" ma ka ʻili o nā huahana, i kumu ʻia e ka ʻokoʻa o nā waiwai a me nā ʻano o ka ʻili o nā huahana a me nā mea ʻē aʻe, a hana ia i kahi ʻili ʻili e hiki ke wehe ʻia.
Ke koʻikoʻi ka lamination, ua hana ʻia ka ʻāpana keʻa holoʻokoʻa i nā papa like ʻole, ʻaʻole i hoʻoheheʻe ʻia. Ke ʻike ʻole ʻia nā hemahema, hiki i ke ʻano o nā huahana ke kūpono i nā koi, akā e uhaʻi i nā waiwai mechanical o nā huahana.
Ke kumu:
ʻElua kumu nui no ka lamination. ʻO ka mea mua, ʻo ia ke hui hewa ʻia nā ʻano mea maka ʻelua. E lawe ʻia nā mea maka ʻelua i loko o ka pahu i ka manawa like ma lalo o ke kaomi. Eia nō naʻe, inā ʻaʻole hiki ke hoʻoheheʻe ʻia ka ʻōpala i ka wā e maʻalili ʻia, e like me nā papa ʻokoʻa i kaomi ikaika ʻia e hana i nā huahana.
ʻO ka lua: inā e hoʻoheheʻe ʻia ke anuanu e hele i ka puka haiki, e hana ʻia ke koʻikoʻi shear. ʻO ke koʻikoʻi ʻāwīwī kiʻekiʻe ke kumu e hoʻoheheʻe ʻia ka papa hoʻoheheʻe ma mua ʻaʻole hiki ke hoʻohui ʻia.
ʻO ka pilikia o ka hui ʻana:
ʻO kahi mea pono e hoʻomaopopo ʻia ʻo ia ka hopena o kekahi mau mea maka i hui pū ʻia i ka hopena kemika ikaika, e like me PVC a me Avetal ʻaʻole pono e hui ʻia.
Linear kala
He ʻano ʻano kūloko wale nō paha ka laina Sliver, akā hiki ke hoʻonui ʻia i ka ʻili holoʻokoʻa ke koʻikoʻi.
E hoʻopilikia ka linear kālā i ke ʻano o nā huahana a hōʻino pū i nā waiwai mechanical o nā huahana.
Ke kumu:
ʻO nā kumu ʻelua ma lalo nei ke kumu o ka linear kālā:
Pulu ka mea maka a ʻo kekahi o lākou e komo i ka mahu i ka lewa. Inā pulu loa ka mea maka, hiki ke hana ʻia ka mahu ma lalo o ka wela kiʻekiʻe a me ke kaomi kiʻekiʻe o ka barela. Wehe kēia mau mahu ma ka ʻili o ka huahana a hana i nā kaha kala.
Ua pōʻino ka hoʻoheheʻe ʻana i ka wela a hoʻohua i ka pōʻino kūloko. E ālai ʻia ke kinoea hoʻoheheʻe ʻia ma luna o ka ʻili o ka lepo a hoʻoulu i nā kaha ma ka ʻili o nā huahana.
ʻAʻole kēia i ʻoi aku ka ʻino e like me ka hoʻohaʻahaʻa. I ka lōʻihi o ke kiʻekiʻe o ka wela o ka heheʻe ʻana a i ʻole e hoʻokau ʻia i ke koʻikoʻi shear i ka wā o ka plasticization a i ʻole ke komo ʻana i loko o ka mold, hiki paha kēia.
ʻAlohi/aka
Pono e like ka hoʻopau ʻana o ka ʻili o nā huahana e like me nā molds. Ke ʻokoʻa ka pau ʻana o ka ʻili o ʻelua, ua ʻike ʻia nā pōʻino ʻoniʻoni.
E pōʻeleʻele ka ʻili i ka wā i loaʻa mai ai nā kīnā, a ʻo ka ʻili ʻōpala he laumā a ʻālohilohi.
Ke kumu:
ʻO nā kumu o ka ʻālohilohi/aka:
Kahe ʻole ka hehee ʻana a i ʻole ka haʻahaʻa o ka wela o ka ʻili o ka poʻi, ʻo ka hopena ʻaʻole hiki ke hoʻopaʻa ʻia ka pau ʻana o ka ʻili i ka wā e hoʻoheheʻe ʻia ai nā mea.
I ka wā e paʻa ai ke kaomi, ʻaʻole kiʻekiʻe ke kaomi i loko o ka lua e hoʻopili ai ka mea i ka ʻili o ka mold i ke kaʻina hoʻoluʻu, e waiho ana i nā hōʻailona shrinkage.

Nā kaila lele
Hiki ke loaʻa nā kaha kahe ma ka ʻili o nā huahana ma nā ʻano he nui. ʻO ka maʻamau, e hana ia i wahi aka.
ʻAʻole hana nā kaha kahe i kahi embossing a i ʻole ke kaumaha ma ka ʻili o nā huahana, ʻaʻole hiki ke ʻike ʻia me nā manamana lima. Ua kapa ʻia kēia hemahema he kaha kauo, ʻuhane, a me nā aka.
Ke ʻike ʻia nā kaha kahe, e hoʻopuka ʻo ia i nā grooves, a waiho i nā hemahema e like me nā kaha ma ka ʻili o nā huahana.
Ke kumu:
Hiki ke loaʻa nā kaha kahe i ka wā:
He haʻahaʻa ka flowability o ka heheʻe a i ʻole ka haʻahaʻa o ka wela o ka ʻili, ka hopena i ka nui o ke kahe ʻana o ka plastic i ke kaʻina hana hoʻopiha piha.
I ka hoʻopiha piha ʻana, kahe ka hehee me ke kūpaʻa, hiki ke kumu ʻia e ka ʻili ʻole o ka make, nā hōʻailona a i ʻole nā hiʻohiʻona i paʻi ʻia ma ka ʻaoʻao make, a i ʻole ka hoʻololi ʻana o ke kahe kahe ʻana i ka wā o ka hoʻopiha ʻana.
Laina hui
Hoʻokumu ʻia ka laina hoʻohui i ka wā e hui ai nā mua hehee ʻelua i ka wā o ka hoʻopiha piha ʻana, a e ʻike ʻia ma ka ʻili o ka huahana e like me kahi laina.
ʻO ka laina hui e like me ka laina pohā ma ka ʻili o nā huahana, ʻaʻole maopopo ke ʻike.
I ka hoʻolālā ʻana i nā mole, ʻaʻole hiki ke ʻalo ʻia kekahi mau laina hoʻohui i ʻike ʻia. I kēia hihia, e hoʻopōkole i ka laina hui e like me ka hiki ke pale i ka ikaika a me ke ʻano o nā huahana.
Ke kumu:
Nui nā kumu o ka hoʻoheheʻe ʻana i mua. ʻO ke kumu nui loa, ʻo ia ke kahe hehee ʻana ma nā ʻaoʻao o ka mold core. I ka hui ʻana o nā mea ʻelua, hana ia i nā laina hui. Pono ke kiʻekiʻe o ka wela o nā mea hoʻoheheʻe ʻelua e hiki ai iā lākou ke hui pū me ka maikaʻi, a ʻaʻole pili i ka ikaika a me ke ʻano o nā huahana.
Inā ʻaʻole hiki i nā mea hoʻoheheʻe ʻelua ke hui pū ʻia, e hana ʻia nā hemahema.
Nā kumu o nā hemahema:
He ʻoi aku ka mānoanoa a me ka lahilahi o ka ʻāpana, a ʻokoʻa ka holo kahe o ka heheʻe, i ka wā e kahe ai ka hoʻoheheʻe ʻana ma ka ʻāpana lahilahi o ka ʻōpala, ua haʻahaʻa ka mahana.
He ʻokoʻa ka lōʻihi o kēlā me kēia kukini. E maʻalili ka poʻe holo loner.
ʻAʻole lawa ka paʻi ʻana o ka lua e hiki ai ke hoʻoheheʻe ʻia i ka hoʻoheheʻe ʻana i ka wā o ka paʻa paʻa ʻana.
ʻO nā ʻōhū i koe e hiki ʻole ai i ka mua hehee ke hoʻokuʻi, e alakaʻi pū ai i ke ahi.
ke ahi
Ua like ke ahi me ka pana pōkole, akā me nā ʻaoʻao mae ʻole a me ka ʻala ʻala iki. E ʻike ʻia nā wahi ʻeleʻele kalapona ma ka huahana, i ka wā e koʻikoʻi ai ke ʻano, me ka ʻala o ka ʻā ʻana o ka plastic.
Inā ʻaʻole i hoʻopau ʻia nā hemahema, loaʻa pinepine ka waiho ʻeleʻele ma ka ʻōpala. Inā ʻaʻole nānā koke ʻia ke kinoea a i ʻole nā mea aila i hana ʻia ma ke puhi ʻana, hiki iā lākou ke pani i nā lua ea. Loaʻa ke ahi ma ka hopena o ke ala.
Ke kumu:
Hoʻomaka ʻia ke ahi ma muli o ka hopena kuni kūloko. Ke piʻi nui ke kaomi i ka lewa i loko o ka manawa pōkole loa, e piʻi aʻe ka mahana a hoʻopau i ke ahi. Wahi a ka ʻikepili i hōʻiliʻili ʻia, hiki i ka hopena o ka hoʻoulu ʻana i loko o ke kaʻina hana hoʻoheheʻe injection ke hana i ka wela kiʻekiʻe a hiki i 600 degere.
Hiki ke hana ʻia ke ahi inā:
ʻO ka wikiwiki ka hoʻopiha piha ʻana i ka ea ʻaʻole hiki ke hoʻokuʻu ʻia ka ea mai ka lua o ka mold, a hoʻopuka i nā ʻeleʻele ea ma muli o ka poloka o ka plastic e komo mai ana, a alakaʻi i ka hopena o loko ma hope o ke kaomi ʻana.
Ua ālai ʻia nā puka ea a ʻaʻole maʻalahi ka ea.
Pono e hoʻokuʻu ʻia ka ea i loko o ka ʻōpala mai nā lua ea. Inā pili ka ea i ke kūlana, ka helu, ka nui a i ʻole nā hana, e noho ka ea i loko o ka ʻōpala a alakaʻi i ke ahi. ʻO ka ikaika clamping mold nui e alakaʻi i ka ventila maikaʻi ʻole.
ʻO ka hoʻoiho
ʻO ka hoʻohaʻahaʻa e pili ana i nā puka liʻiliʻi ma ka ʻili o nā huahana.
Ke liʻiliʻi nā hemahema, ʻaʻole kūlike ka ʻili o nā huahana. Ke koʻikoʻi, hāʻule ka ʻāpana nui o nā huahana. Loaʻa pinepine nā huahana me nā pio, nā lima a me nā protrusions i nā hemahema shrinkage.
Ke kumu:
ʻO ka emi ʻana ma muli o ka emi ʻana o nā mea maka i ka wā hoʻoluʻu.
Ma ka mānoanoa o nā huahana (e like me ka arch), he haʻahaʻa ke ʻano kumu o nā mea, no laila e hiki mai ka emi ʻana ma mua o ka ʻili o ka ʻili, kahi e hoʻoulu ai i ka ikaika contraction i loko o ka mea maka, a huki i ka ʻaoʻao o waho i loko o ke kaumaha. e hana i ka emi ana.
Hiki ke emi i nā kūlana penei:
ʻOi aku ka haʻahaʻa o ke kaomi i loko o ka lua mold ma mua o ka ikaika i hana ʻia mai ka emi ʻana o nā mea maka i ke kaʻina hoʻoluʻu.
ʻAʻole lawa ka manawa pressurization o ka mold cavity i ka wā o ke kaʻina hana hoʻoluʻu, ka hopena i ka holo ʻana o ka waiwai maka i waho o ka lua mai ka puka.
ʻAʻole lawa ka hiki ke hoʻopaʻa i ka mea maka i ka wā o ka hoʻoheheʻe ʻana a me ka hoʻopaʻa paʻa ʻana i ke kahua no ka mea ua hoʻihoʻi ʻia ka wili ma mua o ka hoʻokomo ʻia ʻana o ka mea maka.
ʻOi aku ka liʻiliʻi o nā ʻāpana ʻāpana o nā ʻīpuka a me nā kukini ma mua o ka mānoanoa o nā huahana, ʻo ia hoʻi, ua maloʻo nā puka ma mua o ke kaʻina extrusion huahana.
Oe
Hōʻike ʻia nā ʻūhā ʻūlū ma ke ʻano o nā ʻōpū o ka ea, hiki ke loaʻa maʻalahi ma nā huahana alohilohi. Hiki ke ʻike ʻia ma ka ʻāpana keʻa o nā huahana opaque.
Ke kumu:
ʻO nā ʻōhū ea ka ʻāpana ʻāʻī o nā huahana, i hana ʻia i ka wā e emi ai ka mea maka i ka wā o ka hoʻoilo.
E like me ka emi ʻana, ʻo ka loko o ka mea maka e hana i ka ikaika contractile. ʻO ka mea ʻokoʻa, ua hoʻopaʻa ʻia ka helehelena waho o nā huahana i ka wā i hoʻokumu ʻia ai nā ʻōpū, ʻaʻohe hāʻule, no laila ua hoʻokumu ʻia nā ʻōhū hollow.
ʻO nā kumu o ka puʻupuʻu ua like ia me nā kumu o ka emi ʻana, e like me:
ʻAʻole kūpono ka paʻi ʻana o ka lua
ʻAʻole lawa ka manawa pressurization o ka lua
ʻO ka nui o ka mea kukini a me ka puka he liʻiliʻi loa
Hoʻopuʻi ʻana i nā māka
ʻO nā kaha hoʻopuʻi e pili ana i ka ʻāpana wili e kū pono ana i ka puka. ʻAʻole pili wale nā hōʻailona spraying i ke ʻano o nā huahana, akā pili pū kekahi i ka ikaika o nā huahana.
Ke kumu:
Hoʻokumu ʻia nā hōʻailona ma muli o ke kahe hehee ʻana i waho o ka mana i ka wā o ka hoʻopiha piha ʻana.
Hoʻokomo ka plastic i hoʻoheheʻe ʻia i loko o ka poʻi ma lalo o ke kaomi nui. Inā ʻoi aku ka kiʻekiʻe o ka wikiwiki o ka hoʻopiha ʻana, e hoʻokuʻu ʻia ka plastik mai ka puka hāmama o ka lua polū, a laila e hoʻi koke a maʻalili. I kēlā manawa, hoʻokumu ʻia nā kaula, kahi e pale ai i ka palaka i hoʻoheheʻe ʻia e komo i loko o nā puka.
ʻO ke kumu nui o ka pīpī ʻana i nā māka ʻo ke kūlana kūpono ʻole o nā ʻīpuka a i ʻole ka hoʻolālā ʻana o ka puka. ʻO kēia mau kūlana ʻelua e hōʻeha i ke kūlana o nā hemahema:
ʻO ka wikiwiki hoʻopiha piha
ʻAʻohe kahe hoʻoheheʻe i ka wā e hoʻopiha ai i ka poʻi