6 Wamba Pulasitiki jekeseni Akamaumba Zolakwika Ndi Mayankho
6 Wamba Pulasitiki jekeseni Akamaumba Zolakwika Ndi Mayankho
Ndi wamba kuti pamene ntchito ndi pulasitiki yopangira jekeseni zovuta zambiri zimabuka. Komabe, musachite mantha, zambiri mwazovutazi ndizofala komanso zimathetsedwa mosavuta. Apa tiyika mndandanda, wokhala ndi mayankho osiyanasiyana oti titenge.
Vuto #1: Mphamvu ya Dizilo
Choyamba, tikutanthauza chiyani ndi mphamvu ya dizilo?
Ndi pamene zizindikiro zakuda kapena zopsereza zimawonekera pa gawo lopangidwa.
Izi zimakhala zovuta, nthawi zambiri, chifukwa zigawozo sizimadzadzidwa mokwanira m'madera amenewo.
Izi zimachitika chifukwa cha mpweya wabwino, mpweya sungathe kuthawa kapena suyenda mofulumira kumakona, kusiya kutentha kumakanikizidwa ndikufulumizitsa kufika pamiyeso yokwera kwambiri.
Anakonza
Ikani malo olowera kumalo komwe kutentha kumasiyanasiyana ndikuchepetsa liwiro la jekeseni.
Vuto Lachiwiri: Nkhungu Idzaze Mozengereza Kwambiri
Ndikofunikira kwambiri kuti gawo lokakamiza la Chalk lichitike panthawi yoyenera.
Zikachitika posachedwa, kupanikizika kumakhudzidwa, zomwe zimapangitsa kuti zikhale zosatheka kudzaza patsekeke.
Koma, ngati zichitika mofulumira kwambiri, zimabweretsa kukwera kwakukulu komwe kungawononge nkhungu.
Anakonza
- Wonjezerani kutentha kwa zinthuzo.
- Wonjezerani kutentha kwa nozzle.
- Wonjezerani kapena kuchepetsa kutentha kwa nkhungu.
- Wonjezerani kuthamanga kwa jekeseni.
Vuto #3: Peel ya Orange
Ndi vuto lomwe limayambitsidwa ndi kusapukuta bwino kwa nkhungu.
Zimatchedwa chifukwa pamwamba pa zidutswa za pulasitiki zimakhala ndi mawonekedwe ofanana ndi peel ya lalanje.
Itha kupanga zolakwika zosafunikira monga ma ripples ndi ma pitting, zomwe zimakhudza mtundu wa chinthu chomaliza.
Anakonza
- Kupukuta koyenera kwa nkhungu.
- Ngati kuli kofunikira, sinthani zinthuzo kuti zikhale zoyenera pagawo lobayo.
Vuto #4: Zizindikiro Zolowa ndi Mipata
Zizindikiro zolowera m'madzi zimayamba chifukwa cha kulimba ndi kupindika kwa kunja osati mkati.
Kodi tikutanthauza chiyani pamenepa?
Kunja kukakhala kolimba, kutsika kwamkati kwazinthu kumachitika, kuchititsa kuti nyanjayi igwetse pansi ndikupangitsa kutsika.
Mabowowo amayambanso ndi chodabwitsa chomwecho, koma amawonekera ndi dzenje lamkati.
Anakonza
Itha kuthetsedwa pogwiritsa ntchito zigawo zoonda komanso makulidwe ofanana.
Vuto #5: Nkhungu Ili Ndi Chilema Pakumaliza Kapena Kupanga.
Izi zimachitika pamene nkhungu ili ndi zolakwika kapena kupunduka, zomwe zimapangitsa kuti zotsatira zomaliza zisakhale monga momwe zimayembekezeredwa, zomwe zimayambitsa mavuto ndikuchedwa kupanga.
Anakonza
- Onjezerani chophimba pamwamba pa nkhungu.
- Pogaya pamwamba pa nkhungu.
- Kusintha nkhungu pamapeto pake.
Vuto # 6: Pali mitundu yoyipa pambaliyi.
Kujambula kwa zidutswa zomwe zimayenera kupangidwa ndi sitepe yovuta, popeza kukongola kwa chidutswacho, chizindikiritso ndi ntchito za kuwala zimadalira ndondomekoyi.
Choncho, ngati mtundu ndi kuika kwake sikusankhidwa bwino, zotsatira zake sizidzakhala monga momwe zikuyembekezeredwa, choncho, chidutswacho chikhoza kuonedwa ngati chiwonongeko.
Anakonza
Utoto ungakhale wosayenerera. Yesani kusintha mtundu wa utoto kapena ndende.
Kuti mudziwe zambiri za wamba pulasitiki jekeseni akamaumba zolakwika ndi njira,mutha kuyendera ku Djmolding pa https://www.djmolding.com/solutions-to-common-molding-defects-of-injection-molding/ chifukwa Dziwani zambiri.