Kuqhelekile ukuba xa usebenza kunye yokufakelwa kwiplastiki ubunzima obuninzi buvela. Nangona kunjalo, akufanele wothuke, uninzi lwezi ngxaki zixhaphakile kwaye zisonjululwa ngokulula. Apha siza kubeka uluhlu, kunye nenani ezahlukahlukeneyo zezisombululo zokuthatha.
Ingxaki #1: Impembelelo yeDizili
Okokuqala, sithetha ukuthini ngempembelelo ye-diesel?
Kuxa amabala amnyama okanye ukutsha kuvela kwindawo ebunjiweyo.
Oku kunzima, kwiimeko ezininzi, kuba iinxalenye azigcwaliswanga ngokupheleleyo kwezo ndawo.
Esi siphumo sibangelwa kukungena komoya okungahambi kakuhle, umoya awukwazi ukubaleka okanye awuhambi ngokukhawuleza ukuya kwiikona, ukushiya ubushushu buxinzelelwe kwaye bukhawuleze ukuya kumazinga aphezulu kakhulu.
isisombululo
Beka izithuba kwiindawo apho ukutshisa kwahluka kwaye unciphise isantya sokutofa.
Ingxaki yesi-2: Ukungunda kuzaliswa kancinane
Kubaluleke kakhulu ukuba inqanaba loxinzelelo lwezixhobo zenzeke ngexesha elifanelekileyo.
Ukuba kwenzeka ngokukhawuleza, uxinzelelo oluchaphazelekayo, okwenza kube nzima ukuzalisa ngokupheleleyo i-cavity.
Kodwa, ukuba iyenzeka ngokukhawuleza kakhulu, ikhokelela kwi-spike yoxinzelelo enokonakalisa umngundo.
isisombululo
- Yandisa iprofayili yeqondo lokushisa kwizinto eziphathekayo.
- Yandisa ubushushu bombhobho.
- Ukwandisa okanye ukunciphisa iqondo lobushushu kubumba.
- Yandisa uxinzelelo lwenaliti.
Ingxaki #3: I-Orenji Peel
Yingxaki ebangelwa kukumenyezwa kakubi komngundo.
Kubizwa ngokuba ngenxa yokuba umphezulu weziqwenga zeplastiki ufumana ukuthungwa okufana ne-peel ye-orenji.
Isenokwenza iziphene ezingafunekiyo ezinje ngamariphu kunye nemingxuma, echaphazela umgangatho wemveliso yokugqibela.
isisombululo
- Ukugulisa ukungunda ngokuchanekileyo.
- Ukuba kuyimfuneko, tshintsha izinto eziphathekayo ukuze zilungele inxalenye etofweyo.
Ingxaki #4: Amanqaku atshoneyo kunye neZikhewu
Amanqaku atshoneyo abangelwa kukuqina kunye nokucutheka komphezulu ongaphandle kunomgangatho ongaphakathi.
Sithetha ukuthini ngoku?
Emva kokuba umphezulu wangaphandle uqina, ukucutheka kwangaphakathi kwezinto kwenzeka, okubangela ukuba unxweme lucinezele ngaphantsi komhlaba kwaye lubangele ukuhla.
Imingxuma nayo ibangelwa yinto efanayo, kodwa izibonakalisa ngomngxuma wangaphakathi.
isisombululo
Inokusombululwa ngokusebenzisa amacandelo amancinci kunye nobukhulu obufanayo.
Ingxaki #5: Umngundo unesiphako ekugqibeni okanye ekuyilweni.
Oku kwenzeka xa isikhunta sinesiphoso okanye ukukhubazeka, okubangela ukuba umphumo wokugqibela ungabi njengoko kulindeleke, kubangela iingxaki kunye nokulibaziseka kwemveliso.
isisombululo
- Yongeza i-coat surface kwi-mold.
- Gaya ubuso besikhunta.
- Shintsha isikhunta ekugqibeleni.
Ingxaki #6: Kukho umbala ombi kwicala.
Umbala weengcezu eziza kubumba linyathelo elibalulekileyo, ekubeni ubuhle beqhekeza, ukuchongwa kunye nemisebenzi ye-optical kuxhomekeke kule nkqubo.
Ngoko ke, ukuba umbala kunye nogxininiso lwawo alukhethwanga ngokuchanekileyo, umphumo awuyi kuba njengoko kulindeleke, kwaye ngoko ke, isiqwenga sinokuthathwa njengenkunkuma.
isisombululo
Idayi isenokungafaneleki. Zama ukutshintsha uhlobo lwedayi okanye ugxininiso.
Ukufumana okungakumbi malunga ne iziphene eziqhelekileyo zokubumba inaliti yeplastiki kunye nezisombululo,ungandwendwela Djmolding e https://www.djmolding.com/solutions-to-common-molding-defects-of-injection-molding/ ngolwazi olungakumbi.